Abstract
We report on a systematic study of the thickness dependence of the optical properties of La0.7 Sr0.3 Mn O3 thin films epitaxially grown on a LaAl O3 substrate. The x-ray powder-diffraction data indicate that the c -axis lattice constant is enhanced with decreasing the film thickness due to the compressive strain in the film plane produced by lattice mismatch. Magnetization curves show a decrease of the Curie temperature (TC) for decreasing thickness of films. Optical reflectance and transmittance measurements provide evidence that the position of Mn-O stretching mode shifts toward low frequency and the energy of the charge-transfer transition between O 2p and Mn 3d states increases with the decrease of film thickness. Most importantly, an analysis of the small-polaron absorption in the mid-infrared region shows that the polaron binding energy increases with decreasing the film thickness, suggesting that the strain dependence of TC mainly results from the strain-induced electron-phonon coupling.
| Original language | English |
|---|---|
| Article number | 113528 |
| Journal | Journal of Applied Physics |
| Volume | 97 |
| Issue number | 11 |
| DOIs | |
| State | Published - 2005 |
| Externally published | Yes |
Fingerprint
Dive into the research topics of 'Thickness-dependent optical properties of La 0.7 Sr 0.3 Mn O3 thin films'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver