Enhanced structural integrity of Laser Powder Bed Fusion based AlSi10Mg parts by attaining defect free melt pool formations

  • M. Saravana Kumar*
  • , Che Hua Yang
  • , Muhammad Umar Farooq*
  • , V. Kavimani
  • , Adediran Adeolu Adesoji*
  • *此作品的通信作者
  • National Taipei University of Technology
  • University of Leeds
  • Karpagam Academy of Higher Education
  • Landmark University
  • CSIR - National Metallurgical Laboratory
  • University of Johannesburg

研究成果: 期刊稿件 › 文章 › 同儕審查

27 引文 斯高帕斯(Scopus)

摘要

This research aims to fabricate an AlSi10Mg parts using Laser Powder Bed Fusion technique with enhanced structural integrity. The prime novelty of this research work is eliminating the balling and sparring effects, keyhole and cavity formation by attaining effective melt pool formation. Modelling of the Laser Powder Bed Fusion process parameters such as Laser power, scanning speed, layer thickness and hatch spacing is carried out through Complex Proportional Assessment technique to optimize the parts' surface attributes and to overcome the defects based on the output responses such as surface roughness on scanning and building side, hardness and porosity. The laser power of 350 W, layer thickness of 30 µm, scan speed of 1133 mm/s, and hatch spacing of 0.1 mm produces significantly desirable results to achieve maximum hardness and minimum surface roughness and holding the porosity of < 1%. The obtained optimal setting from this research improves the structural integrity of the printed AlSi10Mg parts.

原文英語
文章編號16672
頁(從 - 到)16672
期刊Scientific Reports
卷13
發行號1
DOIs
出版品狀態已出版 - 04 10 2023
對外發佈是

文獻附註

© 2023. Springer Nature Limited.

UN SDG

此研究成果有助於以下永續發展目標

  1. SDG9 工業、創新基礎建設
    SDG9 工業、創新基礎建設

指紋

深入研究「Enhanced structural integrity of Laser Powder Bed Fusion based AlSi10Mg parts by attaining defect free melt pool formations」主題。共同形成了獨特的指紋。

引用此