摘要

In this study, the long-term resistance of Ce-TZP/Al2O3 specimens to hydrothermal treatment is evaluated in terms of their microstructure. Treatment of the specimens is carried out in an autoclave with water at 134°C for up to 360 h. The biaxial strength and Weibull modulus of the specimens remains unchanged after 120 h of hydrothermal treatment, and their pseudo-plasticity is preserved. However, after 360 h of hydrothermal treatment the biaxial strength decreases by 12% and the Weibull modulus is also decreased. The transformation surface layer is observed through scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The thickness of the transformation layer can be estimated only through TEM analysis, revealing minimal microcrack formation at the surface layer. For comparison, several Y-TZP specimens are also prepared. After 24 h of hydrothermal treatment, the monoclinic phase content in the Y-TZP specimen reached 60%, resulting in a 40% decrease in strength. This strength decrease can be attributed to microcrack formation in the surface layer.

原文英語
頁(從 - 到)93-103
頁數11
期刊Journal of Asian Ceramic Societies
卷12
發行號1
DOIs
出版狀態已出版 - 2024
對外發佈是

文獻附註

Publisher Copyright:
© 2024 The Author(s). Published by Informa UK Limited, trading as Taylor & Francis Group on behalf of The Korean Ceramic Society and The Ceramic Society of Japan.

指紋

深入研究「Microstructural characterization of Ce-TZP/Al2O3 after degradation in water」主題。共同形成了獨特的指紋。

引用此